What Makes Concrete Last: Water, Air, Curing and Sulfates
Concrete rarely fails because it was not strong enough on day 28. It wears out because water gets into it, and water brings frost, salt, sulfates and rust with it. Durable concrete is mostly concrete that keeps water out: a dense paste, a well-cured surface, air bubbles where it freezes, the right cement where the soil is aggressive, and enough cover over the steel. This page covers each, with the numbers the American Concrete Institute's building code (ACI 318) uses.
1. Water-cement ratio: the biggest single factor
The water-cement ratio (w/c, or w/cm when fly ash, slag or other cementitious materials are included) is the weight of water divided by the weight of cement. Cement needs only part of the mix water to hydrate; the rest is there to make the concrete workable. When that extra water dries out it leaves tiny connected pores, and those pores are the path for water and salts into the concrete. Lower w/c means a denser paste, higher strength, lower permeability and less shrinkage.
- A w/c of about 0.40 to 0.45 gives dense, low-permeability concrete suited to harsh exposure.
- Around 0.50 is typical of general-purpose mixes.
- Every bucket of water added at the site to make concrete flow easier pushes the ratio up and the durability down. If it needs to flow more, the answer is a water-reducing admixture, not water.
Bagged premix concrete is designed for the water amount printed on the bag. See how much water to mix concrete, and the mix ratio calculator for site-batched proportions.
2. Curing
The surface inch decides how well concrete resists wear, salt and frost, and it is exactly the part that dries first. Concrete kept moist for at least 7 days (3 for Type III cement, longer for blended cements and in cool weather) ends up with a far less porous surface than the same mix left to dry in the sun. See curing concrete.
3. Freezing and thawing: air entrainment
Water expands about 9 percent when it freezes. In saturated concrete that pressure cracks the paste from inside and flakes off the surface (scaling). Air-entraining admixtures fill the paste with evenly spread microscopic bubbles that act as pressure-relief spaces. ACI 318 requires air-entrained concrete for members exposed to freezing and thawing, with more air for smaller aggregate and wetter exposure:
| Maximum aggregate size | Target air, moderate exposure (F1) | Target air, severe exposure (F2, F3) |
|---|---|---|
| 3/8 in (10 mm) | 6.0% | 7.5% |
| 1/2 in (12.5 mm) | 5.5% | 7.0% |
| 3/4 in (19 mm) | 5.0% | 6.0% |
| 1 in (25 mm) | 4.5% | 6.0% |
| 1-1/2 in (37.5 mm) | 4.5% | 5.5% |
The code allows 1 percentage point less air when the specified strength is 5,000 psi or more. Air-entrained concrete should be float and broom finished outdoors, not hard steel troweled.
4. Deicing salts and chlorides
Salt adds to freeze-thaw damage at the surface, and chlorides that reach reinforcing steel start it rusting. Rust takes up more room than steel, so it cracks the concrete along the bar and breaks off the cover. Practical rules for homeowners:
- Do not use deicers on new concrete during its first winter.
- Never use products based on ammonium nitrate or ammonium sulfate (including fertilizers) on concrete; they attack it chemically.
- Shovel early, use sand for grip, and keep drainage working so water does not sit on the slab.
- A penetrating sealer on a cured, dry slab slows water and salt uptake.
5. Sulfate attack
Some soils and groundwaters contain dissolved sulfates, which react with compounds in hardened cement paste and make it expand and crumble. The defense is a low w/cm plus a sulfate-resisting cement: ASTM C150 Type II (moderate sulfate resistance) or Type V (high), the MS and HS designations in ASTM C595 and C1157, or blends with fly ash, slag or other pozzolans that have a record of sulfate resistance. Calcium chloride accelerators are not permitted for severe sulfate exposure. Whether your site has sulfates is answered by a soil test, and the choice of cement is the engineer's.
6. Cover over the reinforcement
Concrete cover is the thickness of concrete between the steel and the outside face. It is the steel's protection against moisture, salt and carbonation. Cover depths for every element are set by the plans and the building code, and they are larger for concrete cast against earth or exposed to weather than for indoor concrete. Steel sitting on the ground at the bottom of a slab, or bars poking near the surface, are a common reason for rust cracking a few years later. Chairs or blocks that hold the steel at the right height are cheap insurance. See reinforced concrete.
7. Alkali-silica reaction
Some aggregates contain reactive silica that reacts with the alkalis in cement paste to form a gel that swells with moisture, causing map cracking years later. It is controlled at the concrete plant through aggregate testing and the use of fly ash, slag or low-alkali cement. If you are batching your own, use aggregate from a supplier who sells it for concrete.
What the code asks for, by exposure
ACI 318 sorts concrete by what it will face and sets a maximum w/cm and a minimum specified strength for each. A selection of the classes (values from ACI 318-19 Table 19.3.2.1, normal-weight concrete):
| Exposure class | Meaning | Max w/cm | Min strength |
|---|---|---|---|
| F1 | Freezing and thawing, limited contact with water | 0.55 | 3,500 psi (24 MPa) |
| F2 | Freezing and thawing, frequent contact with water | 0.45 | 4,500 psi (31 MPa) |
| F3 | Freezing and thawing with water and deicers (reinforced concrete) | 0.40 | 5,000 psi (34 MPa) |
| S1 | Moderate sulfate exposure | 0.50 | 4,000 psi (28 MPa) |
| S2 | Severe sulfate exposure | 0.45 | 4,500 psi (31 MPa) |
| W2 | In contact with water, low permeability required | 0.50 | 4,000 psi (28 MPa) |
| C2 | Reinforced concrete exposed to moisture and chlorides (deicers, seawater) | 0.40 | 5,000 psi (34 MPa) |
Concrete that will not freeze, stays dry, and meets no sulfates or chlorides falls in the mildest classes, with a minimum of 2,500 psi (17 MPa). These figures show why durability and strength travel together: the lower water ratio that keeps water out also raises strength. They are code minimums for engineered work. For a structural element, the exposure class, mix and cover come from the engineer and the local building code; when ordering ready-mix for a driveway in a freezing climate, tell the supplier it is exterior flatwork exposed to freezing and deicers, and they will quote an air-entrained mix to suit.
A durability checklist for a home project
- Order or mix for the exposure: air-entrained concrete outdoors where it freezes.
- Do not add water on site.
- Compact the base and keep water draining away from the slab.
- Keep steel at its specified cover with chairs or blocks.
- Finish after bleed water has gone; float and broom exterior slabs.
- Cure for at least 7 days.
- No deicers the first winter, and never ammonium-based ones.
Safety
Wet concrete is strongly alkaline and can cause chemical burns that may not hurt until hours later. Wear alkali-resistant gloves, long sleeves, long trousers over waterproof boots, and eye protection, even for small jobs, since cement can also cause allergic skin reactions. Wash any splash off promptly with clean water; rinse eyes with clean water for at least 15 minutes and get medical help.